Effects of the evacuation treatment at elevated temperature was investigated to enhance the catalytic activity of Rh/TiO_2 in the early stage of the hydrogenation of CO (CO/H_2=26.7/53.3kp) at 523K. T...he evacuation at 773K after the reduction of RhCl_3/TiO_2 at 673K provided the highest initial activity of 1810mmol CO/g-Rh・h at 523K, both higher or lower evacuation temperatures decreasing the activity to two thirds. The extensive removal of the chlorine involved in the catalyst may allow the most favorable influences of TiO_2 on Rh catalyst through better dispersion and electronic interaction since Rh/TiO_2 prepared from Rh (NO_3)_3 exhibited much inferior activity by the same evacuation treatment.続きを見る
|